LaBr3(Ce) Lanthanum Bromide crystal
Next

LaBr3(Ce) Lanthanum Bromide crystal

FOB Price

Get Latest Price

100 ~ 1000 / Piece

|

1 Piece Minimum Order

Country:

China

Model No:

LaBr3(Ce) Lanthanum Bromide crystal

FOB Price:

100 ~ 1000 / Piece Get Latest Price

Place of Origin:

china

Price for Minimum Order:

100 per Piece

Minimum Order Quantity:

1 Piece

Packaging Detail:

Alumium Housing Encapsulation

Delivery Time:

30days

Supplying Ability:

1000 Piece per Year

Payment Type:

T/T, L/C, PayPal

Product Group :

-

Contact Now
Free Member

Contact Person Ms. jin

xingguang, Beijing, Beijing

Contact Now

Product Description

LBC scintillation crystals (Lanthanum Bromide doped with Cerium chloride) belong to BGRIs potent product, which have the light outputs of 1.3~1.7 times as much as that of NaI:TI, and their decay time is *7ns~*5ns, only 1/*0~1/*0 of NaI:TI. Their energy resolutions are better than all other scintillation crystals known. They can be used for almost fields of nuclear radiation detection because of high performances.

 

Main Properties

Density

4.9~5.3g/cm3

Emission Peak

**0~**5nm

Light Output

**0%~**0% (relative to NaI:TI crystal)

Decay Time

*7~*5ns

Energy Resolution

2.5~3.5% (Cs***7)

LBC scintillation crystals (Lanthanum Bromide doped with Cerium chloride) belong to BGRIs potent product, which have the light outputs of 1.3~1.7 times as much as that of NaI:TI, and their decay time is *7ns~*5ns, only 1/*0~1/*0 of NaI:TI. Their energy resolutions are better than all other scintillation crystals known. They can be used for almost fields of nuclear radiation detection because of high performances.

 

Main Properties

Density

4.9~5.3g/cm3

Emission Peak

**0~**5nm

Light Output

**0%~**0% (relative to NaI:TI crystal)

Decay Time

*7~*5ns

Energy Resolution

2.5~3.5% (Cs***7)

 

Country: China
Model No: LaBr3(Ce) Lanthanum Bromide crystal
FOB Price: 100 ~ 1000 / Piece Get Latest Price
Place of Origin: china
Price for Minimum Order: 100 per Piece
Minimum Order Quantity: 1 Piece
Packaging Detail: Alumium Housing Encapsulation
Delivery Time: 30days
Supplying Ability: 1000 Piece per Year
Payment Type: T/T, L/C, PayPal
Product Group : -

Send a direct inquiry to this supplier

To:

Ms. jin < beijing glass research institute >

I want to know: