Looks like you are not TradeKey.com's Member yet. Signup now to connect with over 10 Million Importers & Exporters globally.
Join Now, its Free |
BOOK A CALL
Book Call On Your Favorite Time

By Signing Up. I agree to TradeKey.com Terms of Use, Privacy Policy, IPR and receive emails related to our services

Contact Us
product
Prev
Ordinary Glass Frosting Powder
Next

Ordinary Glass Frosting Powder

FOB Price

Get Latest Price

|

- Minimum Order

Country:

China

Model No:

ST-101

FOB Price:

Get Latest Price

Place of Origin:

-

Price for Minimum Order:

-

Minimum Order Quantity:

-

Packaging Detail:

-

Delivery Time:

-

Supplying Ability:

-

Payment Type:

-

Product Group :

-

Contact Now

Contact Person bai

Songtao road, Shanghai, Shanghai

Contact Now

Product Specification

Product Description

Common Glass Frosting Powder ST***1 can frost Sodium-Calcium-Silicon glass such as lamp glass, flat glass, bottles, arts ***** ST***1 is based on industrial grade Hydrochloric Acid. It is a new type environment-friendly powder that allows a better recycling . Stable and easy to use the powder makes your glass appears softer and white.


Frosting Operation >> Preparation of the Frosting Solution
·Mature the Frosting solution at least *4 hours before use

·The ratio of powder ST***1 to Hydrochloric Acid
 (≥*1) is 1:0.*0
·Keep the powder in a plastic container, slowly pour Hydrochloric
  Acid in, and keep stirring the solution evenly. Finally, cover
  the container.
·Keep maturation over *4 hours before use (The longer, the better)
·The newly-prepared solution is too thick, and its temperature
 will fall down slowly, so don"t apply it until it comes back to
 be normal in temperature and thickness.

Frosting Operation >>Frosting Process
·Constantly stir the matured solution to be even completely

·Dip the clean glass wares into the solution for ****0 seconds

· Take out the etched glass to drop for ****0 seconds

·In the beginning, the solution is fairly thick. However the
 etching time should be longer when the solution becomes less
 thick after etching for some time. 
·The frosting time varies with the temperature and chemical
 compositions
·For dirty glass, use *5 Hydrochloric Acid to wash

Frosting Operation >>Wash Process & Dry
 · Rinse and wash the frosted glass wares under the running water
· Dip the glass into the ***0 diluted Hydrochloric Acid for ****0
 seconds to make brasive parparticles on the glass easy to
 remove
·Rinse and wash the glass again under the running water
 and dry it with air for package

Country: China
Model No: ST-101
FOB Price: Get Latest Price
Place of Origin: -
Price for Minimum Order: -
Minimum Order Quantity: -
Packaging Detail: -
Delivery Time: -
Supplying Ability: -
Payment Type: -
Product Group : -
Ordinary Glass Frosting Powder

Send a direct inquiry to this supplier

To:

bai < torlin chemicals >

I want to know: